CNLITE Ecofriendly Gold Leaching Reagent
After the raw ore is piled up or put into the pool, the alkalinity should be adjusted to the pH of 11#177;1. Dosage: The dosage of CNLITE gold dressing agent can refer to the dosage of sodium cyanide. Its dosage is about to parts per thousand (g of reagent/ton of ore).